Product name : 14-4PH Alloy Round Bar
Grades : 14-4PH
Processing methods : Peeled, Milled, Cold working, etc.
Heat treatment condition : quenched and tempered, etc.
Surface : Grinding, Centreless Ground, etc
Available Shapes : Round bar, Flat bar, Forging piece,etc
Price Term : Ex-work, FOB, CIF, CFR, DDU etc.
14-4PH Alloy Round Bar 14-4PH Superalloy
Description
14-4PH Alloy Round Bar 14-4PH Superalloy is High temperature alloys and other special alloys
All of 14-4PH Alloy Round Bar 14-4PH Superalloy conform to Military standard, nuclear power. 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.
Products Details
14-4PH Alloy Round Bar 14-4PH Superalloy
| Chemical Composition (weight%): | Mechanical Properties Under Final Heat Treatment: |
| C(%): 0.03 Si(%): 0.75 Mn(%): 0.35 Cr(%): 14.1 Ni(%): 4.25 Mo(%): 2.38 Co(%): — W(%): — Al(%): — Cu(%): 3.25 Ti(%): — Other(%): Nb 0.25,N 0.02 | TS, σb/≥MPa: 268 YS, σ0.2≥/MPa: 782 EL, δ 5≥(%): 13 Impact, AKV≥/J: 11 |

Applications:
14-4PH Alloy Round Bar 14-4PH Superalloy is often used in the Aerospace, cylinders, gears, hollow shafts, landing gears, marine gas turbine, etc.


FAQ
Q: How do you control the quality?
A: We have professional inspectors to analyze the chemical composition of raw materials and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. You can rest assured that all products you receive from us are reliable.
Q: Do you accept customization?
A: Yes. If you have special requirements for products or packaging, we can make them for you.
Q: Can you accept trial orders?
A: Our MOQ is usually 1 ton. However, if you want to place an order as the start of our cooperation, we can accept smaller quantities at the first time. Of course, after the start, we will have further and longer cooperation.
Q: How do I get samples?
A: Free samples are available for your inspection and testing, DHL/FedEx/UPS accounts can be used for sampling, and the courier fee is borne by you.

|
|
14-4PH Alloy Round Bar 14-4PH Superalloy Images |